Davide is right on target suggesting the use of 3M Acrylic Marine Putty - White, Part No. 051144-05962. Basically it's a fairing compound that dries quickly, and it sands very easily so that it blends effortlessly with those areas surrounding the damaged area. I use it to fill the weave of the fiberglass after laminations, and it's very effective at filling any pinholes that often result from the laminating process.
steveC is offline   Reply With Quote